MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huber Vertex® 100 Magnesium Hydroxide
Categories: Ceramic; Oxide; Magnesium Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Vertex® magnesium hydroxide products provide excellent fire retarding and smoke suppression performance for the thermoplastic and elastomeric compounds. At 330°C, they decompose in an endothermic reaction to form water and magnesium. Vertex 100 is an untreated product that provides superior fire performance and enhanced mechanical properties when used to make fire-rated thermoplastic compounds. Vertex 100 can be used in polyolefins, EPR/EPDM, PVC and certain engineering thermoplastics such as polyamides to make zero-halogen or low-smoke compounds.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.36 g/cc
Particle Size 1.1 µmSedigraph
 1.5 µmLaser Light Scattering
Particle Mesh Size 325 Mesh0.3% Residue
Specific Surface Area 14 m²/gBET
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.5
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.58
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca <= 0.60 %
Free Water 0.30 %
@Temperature 105 °C
Free
Iron, Fe <= 0.080 %
Loss on Ignition(%) >= 31 %
@Temperature 1200 °C
 
Descriptive Properties
ColorWhite
Content<0.3%Chloride
 >99%Mg(OH)2
FunctionalitySmoke Suppression
Market/Application: ThermoplasticsYes
Market/Application: Wire and CableWire & Cable Jacketing - PVC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER794 / 300900

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.