MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® VeroWhite PolyJet Resin White for Rapid Prototyping  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic

Material Notes: Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero PolyJet Resin materials offer great surface finish with improved mechanical properties as compared to our Clear PolyJet Resin (FC720). These parts are built at a layer thickness of 16 microns (0.0006 inch or 0.01524mm) and can produce parts with fine feature detail.

Applications

Vero PolyJet Resins work well for prototypes that require smooth surface finish and high feature detail. These resins offer improvements as compared to our Clear PolyJet Resin such as improved mechanical properties, enhanced visualization of details and edges, improved humidity resistance and better flexural strength. Parts from this material can be chrome plated or used as a master for silicone molds. Typical industries included toys, foot wear, architecture and any industry where feature detail and surface finish our required.

Redeye on Demand has been acquired by Stratasys.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 81
Hardness, Shore D 83
Tensile Strength, Yield 49.9 MPaASTM D638
Elongation at Break 15 - 25 %ASTM D638
Tensile Modulus 2.495 GPaASTM D638
Flexural Yield Strength 74.6 MPaASTM D790
Flexural Modulus 2.137 GPaASTM D790
Izod Impact, Notched 37.5 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CASTM D648
Glass Transition Temp, Tg 58.0 °CDMA (SYSS)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® Clear PolyJet™ FC720 for Rapid Prototyping
Stratasys® VeroBlack PolyJet™ FC870 for Rapid Prototyping
Stratasys® VeroBlue PolyJet™ FC840 for Rapid Prototyping
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer
Stratasys® PolyJet™ TangoBlack™ FC970 Rapid Prototyping Material

PSTRAT998 / 65335

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.