MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: SS4171P model sealer is used to help minimize cure inhibition of addition curing silicone rubber moldmaking material. Properly applied, the model sealer will help to prevent substrates such as sulfur, vinyl, epoxy and soft woods from inhibiting the cure of the silicone rubber moldmaking material. The sealer will allow easy release of the silicone rubber from the model or master.

SS4171P should only be used with addition curing products such as the RTV600 series, TSE34XX series, and RTV800 series products. SS4171P sealer should not be used as a model sealer with condensation cure silicone rubber, as it will act as a bonding agent with this product. Condensation cure products include RTV7888 series, RTV42X series, and RTV430 products.

SS4171P model sealer can also be applied to addition cured silicone rubber as a parting agent in making two-part molds.

It is suggested that a patch test is done before using addition cure silicones. If inhibition is detected, then do a second patch test trying the SS4171P model sealer.

Key Performance Properties:

  • Easy application to patterns
  • One treatment is generally adequate for each wooden pattern
  • Can be used on cured addition cured molds

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.840 g/cc
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point -12.0 °CTag open cup
 
Processing PropertiesOriginal ValueComments
Cure Time 0.5 hourApproximate
 
Descriptive Properties
ColorBlue
Non-Volatile Content14%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials SS4120P Silicone Primer for use with RTV Silicone Adhesive Sealants, Clear
Elkem (Bluestar Silicones) BLUESIL™ V-1062 Hi-Pro Green Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ V 1065 Hi-Pro Green Silicone Rubber
Dow SE 9184 WHITE RTV
Dow SE 738 SILICONE RTV

PGESIL063 / 41054

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.