System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Kumho-Sunny HCG2520FR PC, 20% Glass Fiber Reinforced, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Glass Fiber Filled, Flame Retardant
Material Notes:
HCG2520FR is 20% GF flame retardant PC resin. It has high rigidity and super shape resistance property. HCG2520FR is mainly used in electron & electric parts, etc.
Information provided by Shanghai Kumho Sunny Plastics co, Ltd
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.35
g/cc
ASTM D792
Maximum Moisture Content
0.020
Linear Mold Shrinkage
0.0020
-
0.0040
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength
85.0
MPa
ASTM D638
Elongation at Break
2.5 %
ASTM D638
Flexural Strength
150
MPa
ASTM D790
Flexural Modulus
5500
MPa
ASTM D790
Izod Impact, Notched
100
J/m
@Thickness 3.20 mm
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+15
ohm
IEC 60093
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
145
°C
ASTM D648
Flammability, UL94
V-0
@Thickness 1.60 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
270
-
280
°C
Middle Barrel Temperature
280
-
290
°C
Front Barrel Temperature
290
-
300
°C
Nozzle Temperature
280
-
290
°C
Melt Temperature
240
-
300
°C
Mold Temperature
60.0
-
100
°C
Drying Temperature
100
-
120
°C
Dry Time
3.00
-
4.00
hour
Back Pressure
0.200
-
0.800
MPa
Screw Speed
20
-
80
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PKMSN136 / 280988
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.