MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quadrant Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistance.
  • Thermal stability in the range -76 °C up to +160 °C / -105 °F up to + 356 °F
  • Excellent chemical resistance against highly concentrated chemicals, even for a broad range of alcalines (up to pH 14)
  • Low permeability to liquids, gases and vapors.
  • High elongation at break
  • Excellent impact resistance
  • Good resistance to stress cracking, even with caustic solutions, chlorine and alkaline areas
  • Excellent weather proof and radiation proof
  • Low coefficient of thermal expansion

In January 2016 the Symalit® Fluoroplastics production assets were sold to AGRU Kunststofftechnik GmbH

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.040 %50% RH
Water Absorption at Saturation <= 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ISO 2039-2
Hardness, Shore D 70
Ball Indentation Hardness 65.0 MPaISO 2039-1
Tensile Strength, Yield 30.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
Tensile Modulus 1600 MPaISO 527-1/-2
Flexural Strength 47.0 MPa
Compressive Strength 14.5 MPa
@Strain 1 %
ISO 604
 26.0 MPa
@Strain 2 %
ISO 604
 33.0 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 1100 µm/km
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 180 kJ/m²Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35 - 0.45
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.0e+14 ohm-cmIEC 60093
Surface Resistivity per Square >= 1.0e+13 ohmIEC 60093
Dielectric Constant 2.5
@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm
Dissipation Factor 0.0010
@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.150 W/m-K
Melting Point 240 °CDSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 160 °CContinuous
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CISO 75-1/-2
Flammability, UL94 V-0
Oxygen Index 52 %ISO 4589-1/-2
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
European Food 1935/2004 No
FDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quadrant Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet)
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
Quadrant Symalit® 1000 ETFE unfilled, lining industries (ISO Data)
AGC Fluon® LM-720AP LM-ETFE Fluororesin

PQUADU924 / 130702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.