MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Varcum 29734 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Varcum 29734 is a long-flow, two-step, powdered phenolic resin containing hexamethylenetetramine.

APPLICATION: Manufacture of centerless grinding wheels, cutoff wheels, and wheel segments where resistance to the deteriorating effects of wheel coolants is required.

OVEN CYCLES:Care should be taken in the scheduling of oven cycles and in proper packing of the wheels during oven loading to avoid slumping of the wheels during the oven cycle.

FEATURES: Exhibits excellent grinding action in light-duty and specialty-grinding applications.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Softening Point 69.0 °CCap. Shrink; DCT 4000B
 
Processing PropertiesOriginal ValueComments
Cure Time 105 sec
@Temperature 150 °C
DCT 4001A
 
Descriptive Properties
Hexa0.056DCT 4019A
Inclined Plate Flow90[mm]; DCT 4009A; hot; at 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUMIT732 / 194537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.