MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Sofprene® P Ski Boots 0A0080D30
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Ski Boots, Elastomer-modified polyolefin compound, highly resistant to low temperatures

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D 792
Linear Mold Shrinkage 0.0080 - 0.013 cm/cm
Melt Flow 10 g/10 minASTM 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ASTM D 2240
Tensile Strength 15.0 MPaASTM D412
Elongation at Break 950 %ASTM D412
Flexural Modulus 80.0 MPaASTM D790
Izod Impact Resistance NBASTM D256
Tear Strength 65.0 kN/mASTM D624 C
Compression Set 6.0 %ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 200 °C
 
Descriptive Properties
Featuresavailable in all colors
Surface Appearancetranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Sofprene® P Ski Boots 0D0150D41
Celanese SO.F.TER Sofprene® P Ski Boots 0B0110D40
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
Dow AFFINITY™ SM 8250 Polyolefin Plastomer
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution

PSOFS649 / 162113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.