EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does not contain any slip or antiblocking agent. Applications: - Industrial liners
- Blown film stretch wrap
- Heavy-duty films
- General-purpose blown films for a variety of applications.
Information provided by Equate |