MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow AFFINITY™ PL 1845 Polyolefin Plastomer
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
Thickness 25.0 microns0.984 mil
Melt Flow 3.5 g/10 min
@Load 2.16 kg
3.5 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 527 %527 %
Film Elongation at Break, TD 664 %664 %
Elmendorf Tear Strength MD 178 g178 g
Elmendorf Tear Strength TD 362 g362 g
Elmendorf Tear Strength, MD 7.10 g/micron180 g/mil
Elmendorf Tear Strength, TD 14.5 g/micron368 g/mil
Dart Drop 18.8 g/micron478 g/mil
Film Tensile Strength at Break, MD 45.4 MPa6580 psi
Film Tensile Strength at Break, TD 33.4 MPa4840 psi
 
Optical PropertiesMetricEnglishComments
Haze 0.70 %0.70 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 99.0 °C210 °FSeal initiation temperature
 274 °C525 °FFilm extrusion temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1850 Polyolefin Plastomer
Dow AFFINITY™ KC 8852 Polyolefin Elastomer
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
Dow AFFINITY™ SM 8400 Polyolefin Elastomer

PDW404 / 34473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.