MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kuraray Genestar™ G1302 Nylon, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Abrasion Resistance HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It delivers low friction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/cc
Water Absorption 1.4 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
Melt Flow 46 g/10 min
@Load 2.16 kg,
Temperature 320 °C
ASTM D1238
Spiral Flow 5.50 cm
@Load 750 kg,
Temperature 320 °C
0.5mm diameter
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 47.0 MPaWeld; ASTM D638
 165 MPaASTM D638
Elongation at Yield 0.70 %Weld; ASTM D638
 4.0 %ASTM D638
Flexural Strength 210 MPaASTM D790
Flexural Modulus 9000 MPaASTM D790
Izod Impact, Notched 115 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.3
@Frequency 1e+10 Hz
ASTM D150
Dielectric Strength 30.0 kV/mmASTM D149
Dielectric Loss Index 0.0090
@Frequency 1e+10 Hz
ASTM D150
Comparative Tracking Index >= 600 VASTM UL746A
 
Thermal PropertiesOriginal ValueComments
Melting Point 306 °C
Deflection Temperature at 1.8 MPa (264 psi) 290 °CASTM D648
Glass Transition Temp, Tg 125 °C
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray HYBRAR® Low Rebound Compound # 1
Kuraray HYBRAR® BF3 Three Layer Blown Film
Kuraray HYBRAR® BF2 Three Layer Blown Film
Kuraray HYBRAR® BF1 Three Layer Blown Film
Kuraray HYBRAR® F2 Foam Compound

PKUR118 / 162507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.