MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Polyurethane, Liquid
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.971 - 1.24 g/ccAverage value: 1.08 g/cc Grade Count:101
Water Absorption at Saturation 2.00 - 4.00 %Average value: 3.08 % Grade Count:4
Viscosity 90.0 - 100000 cPAverage value: 3190 cP Grade Count:74
 100 - 15000 cP
@Temperature 45.0 - 82.2 °C
Average value: 2520 cP Grade Count:8
Thickness 102 - 6100 micronsAverage value: 1700 microns Grade Count:5
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cmAverage value: 0.00169 cm/cm Grade Count:34
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 10.0 - 95.0Average value: 59.6 Grade Count:38
Hardness, Shore D 50.0 - 86.0Average value: 79.6 Grade Count:24
Tensile Strength, Ultimate 0.586 - 89.0 MPaAverage value: 32.6 MPa Grade Count:72
Elongation at Break 2.00 - 1000 %Average value: 358 % Grade Count:70
Modulus of Elasticity 0.650 - 3.20 GPaAverage value: 1.91 GPa Grade Count:23
Flexural Yield Strength 32.0 - 115 MPaAverage value: 92.7 MPa Grade Count:21
Flexural Modulus 2.07 - 3.00 GPaAverage value: 2.40 GPa Grade Count:20
Rebound 5.00 - 65.0 %Average value: 38.7 % Grade Count:13
Izod Impact, Notched 0.272 - 4.80 J/cmAverage value: 1.02 J/cm Grade Count:19
Izod Impact, Unnotched 1.17 - 5.02 J/cmAverage value: 3.43 J/cm Grade Count:16
Charpy Impact Unnotched 2.80 - 6.00 J/cm²Average value: 4.60 J/cm² Grade Count:4
Tear Strength 1.21 - 167 kN/mAverage value: 43.5 kN/m Grade Count:43
Taber Abrasion, mg/1000 Cycles 3.00 - 1880Average value: 149 Grade Count:17
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 7.00e+13 - 6.01e+15 ohm-cmAverage value: 2.21e+15 ohm-cm Grade Count:6
Surface Resistance 1.00e+13 - 7.65e+13 ohmAverage value: 3.22e+13 ohm Grade Count:6
Dielectric Strength 15.0 - 18.7 kV/mmAverage value: 16.2 kV/mm Grade Count:6
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 - 160 µm/m-°CAverage value: 131 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 90.0 - 160 µm/m-°CAverage value: 131 µm/m-°C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 67.0 - 195 °CAverage value: 113 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 54.0 - 136 °CAverage value: 85.5 °C Grade Count:12
Vicat Softening Point 94.0 - 245 °CAverage value: 163 °C Grade Count:4
Heat Distortion Temperature 60.0 - 80.0 °CAverage value: 69.7 °C Grade Count:12
Glass Transition Temp, Tg 83.0 - 145 °CAverage value: 105 °C Grade Count:3
Flammability, UL94 V-0Grade Count:9
 
Processing PropertiesOriginal ValueComments
Processing Temperature 18.3 - 93.3 °CAverage value: 42.8 °C Grade Count:26
Mold Temperature 21.1 - 100 °CAverage value: 59.6 °C Grade Count:26
Cure Time 5.00 - 30200 minAverage value: 1910 min Grade Count:52
 15.0 - 1440 min
@Temperature 57.2 - 100 °C
Average value: 434 min Grade Count:17
Pot Life 0.750 - 60.0 minAverage value: 19.2 min Grade Count:46

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Solvay Thornel® Mat VME Carbon Fiber
Overview of materials for Thermoset Polyurethane Foam, Glass Filled

O5000 / 78452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.