PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applications: PS65T20 has been developed especially for the car industry to be used in automotive interior parts including trunk claddings, and other automotive interior applications.Information provided by Borealis AG |