MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond Mastersil 705TC One Component, Thermally Conductive Silicone
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Elastomer, for Thermal Management

Material Notes: Master Bond MasterSil 705TC is a one component, thermally conductive, electrically isolating, high performance silicone for bonding, sealing and coating applications. The material is an off-white colored paste. It cures at ambient temperatures when exposed to atmospheric moisture and is a noncorrosive type silicone. Its most prominent features are excellent thermal conductivity and retention of electrical insulation properties. It has a wide service temperature range of -60°F to +400°F. Its paste-like viscosity is ideal for bonding applications and it adheres well to metals, composites and many plastics.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.46 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 50
Tensile Strength 210 psi
Elongation at Break 70 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 50 Hz
Dielectric Strength 850 kV/in
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 14.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 23.9 °C
unopened container
 
Descriptive Properties
ColorOff-White
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Nitride
Silicon Nitride, HIP-RBSN
Silicon Nitride, HIP-SN
Silicon Nitride, HPSN
Silicon Nitride, RBSN

PMASTB170 / 52327

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.