MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum A413.0-F Die Casting Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium A413.0-F; UNS A14130; AAA413.0-F Die, ISO 3522 AlSi12CuFe and AlSi12Fe. ISO R164 AlSi12, AlSi12Cu, AlSi12CuFe, AlSi12Fe. ISO R2147 , 12Si. Comparable to AC-47100, AC47100, ADC1, ADC 1, ALDC1, ALDC 1; AlA413.0-F
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.66 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 80
Tensile Strength, Ultimate 290 MPa
Tensile Strength, Yield 131 MPa
@Strain 0.2 %
Elongation at Break 3.5 %in 50 mm
Modulus of Elasticity 71.0 GPa413.0-F
Poissons Ratio 0.33
Fatigue Strength 130 MPa
@# of Cycles 5.00e+8
Notch Status unknown, R.R. Moore Test
Machinability 30 %0-100 Scale (100=best)
Shear Modulus 26.7 GPaCalculated
Shear Strength 170 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000440 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/g
CTE, linear 20.4 µm/m-°C
@Temperature 20.0 - 100 °C
 22.4 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.963 J/g-°C
Thermal Conductivity 121 W/m-K
Melting Point 574 - 582 °C
Solidus 574 °C
Liquidus 582 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 1200 - 1400 °F
Casting Temperature 1175 - 1300 °FDie Casting
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 82.9 - 89 %As remainder
Copper, Cu <= 1.0 %
Iron, Fe <= 1.3 %
Magnesium, Mg <= 0.10 %
Manganese, Mn <= 0.35 %
Nickel, Ni <= 0.50 %
Other, total <= 0.25 %
Silicon, Si 11 - 13 %
Tin, Sn <= 0.15 %
Zinc, Zn <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 413.0-F Die Casting Alloy
Aluminum A360.0-F Die Casting Alloy
Aluminum A380.0-F Die Casting Alloy
Aluminum 384.0-F Die Casting Alloy
Aluminum 383.0-F Die Casting Alloy

MAC4130AF / 10086

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.