MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
H.C. Starck HPM 1850W Tungsten High Density Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the customer or in accordance with the drawing as finished machined component.
Our HPM 1700 to HPM 1850 materials provide a solution in a wide range of applications requiring concentrated weight or density in a limited space. These lead-free parts meet legal requirements and recommendations to protect the environment.

Range of Application: Balance weights, radiation protection, vibration absorbers, heat transfer, drilling bars. The mechanical characteristics have to guarantee the stability and strength in any application case.
The absorption of x-ray and gamma radiation is in direct proportion to the density of the shielding material. Tungsten high density composites are more than 1.5 times as effective as lead and provide extremely efficient protection, particularly where space is limited.

Information provided by H.C. Starck.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 18.3 - 18.7 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers <= 340HV 30
Tensile Strength 890 MPa
Tensile Strength, Yield >= 520 MPa
Elongation at Break 12 %
Modulus of Elasticity 380 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000010 ohm-cm
Magnetic Permeability >= 1.05
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.80 µm/m-°C
@Temperature 20.0 - 100 °C
 4.90 µm/m-°C
@Temperature 20.0 - 300 °C
 5.00 µm/m-°C
@Temperature 20.0 - 450 °C
Thermal Conductivity >= 80.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Tungsten, W 97 %Balance - Ni, Fe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAECO® NAECOMET® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal
H.C. Starck HPM 1850 Tungsten High Density Composite
H.C. Starck HPM 1801 Tungsten High Density Composite

NHCST955 / 130844

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.