MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® AX 2677 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Makrolon® is extremely robust, lightweight with glass-like transparency and is impact resistant – even at extremely low temperatures. It has a high dimensional stability and is easily molded, yet has excellent heat resistance with a glass transition temperature of up to 148ºC. Grades are available optimized for lighting, medical and food contact, flame-retardant, impact-modified and glass-fiber reinforced grades. Products made out of polycarbonate boast a long life and allow efficient reusability. Stronger and lighter than glass, polycarbonate also provides energy and CO2 emission savings. Furthermore, it reduces product losses due to breakage during distribution and use. Most post-production waste is mechanically recycled into “recyclate grade” polycarbonate blends.

Mechanical property data for samples at 50% RH.

Information provided by Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/cc
@Temperature 23.0 °C
pellets; ISO 60
Density 1.20 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.12 %
@Temperature 23.0 °C
ISO 62
Water Absorption at Saturation 0.30 %
@Temperature 23.0 °C
ISO 62
Water Vapor Transmission 15.0 g/m²/day
@Temperature 23.0 °C
85% RH, 100µm film; ISO 15106-1
Linear Mold Shrinkage 0.0075 in/in
@Pressure 50.0 MPa
60x60x2 mm; ISO 294-4
Linear Mold Shrinkage, Flow 0.0070 in/in
@Pressure 50.0 MPa
60x60x2 mm; ISO 294-4
Melt Flow 13 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 16700 psi
@Temperature 23.0 °C
ISO 2039-1
Tensile Strength at Break 69.0 MPa50mm/min; ISO 527-1,-2
Tensile Strength, Yield 65.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 50 %50mm/min, complete break; ISO 524-1,-2
 120 %50mm/min, complete break; ISO 524-1,-2
Elongation at Yield 6.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 2400 MPa
@Temperature 23.0 °C
1mm/min, complete break; ISO 527-1,-2
Flexural Strength 98.0 MPa2mm/min; ISO 178
 74.0 MPa
@Strain 3.5 %
2mm/min; ISO 178
Flexural Modulus 2400 MPa
@Temperature 23.0 °C
2mm/min; ISO 178
Flexural Strain at Break 7.1 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
Complete Break; ISO 7391/b.o. ISO 180-A
 70.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
Partial Break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
 NB
@Temperature -60.0 °C
ISO 179-1eU
Charpy Impact, Notched 16.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
ISO 7391/b.o.ISO 179-1eA
 70.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
ISO 7391/b.o.ISO 179-1eA
Puncture Energy 55.0 J
@Temperature 23.0 °C
complete break; ISO 6603-2
 60.0 J
@Temperature -30.0 °C
complete break; ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.00050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 Vsolution B; IEC 60112
 250 Vsolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-Kcross flow; ISO 8302
Hot Ball Pressure Test 135 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °Ccomplete break; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 123 °Ccomplete break; ISO 75-1,-2
Vicat Softening Point 142 °C
@Load 5.10 kg
@ 50°C/h; ISO 306
 143 °C
@Load 5.10 kg
@ 120°C/h; ISO 306
Glass Transition Temp, Tg 142 °C10°C/min; ISO 11357-1,-2
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
Flash Point 480 °CASTM D1929
Ignition Temperature 550 °CSelf Ignition; ASTM D1929
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °Cinjection molding; ISO 294
Mold Temperature 80.0 °Cinjection molding; ISO 294
Injection Velocity 200 mm/secinjection molding; ISO 294
 
Descriptive Properties
Application of Flame from small burner (class)K1,F1DIN 53438-1,-3,method K and F; 2.0mm
Burning Rate (mm/min)passed, ISO 3795>=1.0mm, US_FMVSS
Electrolytic Corrosion (rating)A1, IEC 60426
Puncture Maximum Force (N)5200ISO 6603-2, at 23°C, complete break
 6100ISO 6603-2, at -30°C, complete break

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 6265X Polycarbonate
Covestro Makrolon® ET 3113 Polycarbonate
Covestro Makrolon® 6267X Polycarbonate
Covestro Makrolon® AX 2675 Polycarbonate
Covestro Makrolon® 2807 MAS 167 Polycarbonate

PB095064 / 200134

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.