MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 - 3.10 g/ccAverage value: 2.22 g/cc Grade Count:116
Filler Content 5.00 - 25.0 %Average value: 18.3 % Grade Count:17
Water Absorption 0.000 - 0.100 %Average value: 0.0347 % Grade Count:22
Moisture Absorption at Equilibrium 0.0200 - 0.220 %Average value: 0.0720 % Grade Count:5
 0.0100 - 0.0500 %
@Temperature 50.0 - 50.0 °C
Average value: 0.0300 % Grade Count:2
 0.0100 - 0.0500 %
@Time 173000 - 173000 sec
Average value: 0.0300 % Grade Count:2
Particle Size 25.0 - 800 µmAverage value: 535 µm Grade Count:14
Viscosity 1.00e+13 - 1.00e+15 cP
@Temperature 340 - 380 °C
Average value: 5.05e+14 cP Grade Count:10
Permeability 0.0150Average value: 0.0150 Grade Count:4
Thickness 70.0 - 3180 micronsAverage value: 821 microns Grade Count:17
Linear Mold Shrinkage 0.0140 - 0.0500 cm/cmAverage value: 0.0270 cm/cm Grade Count:20
Melt Flow 3.50 - 5.50 g/10 minAverage value: 4.38 g/10 min Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50.0 - 75.0Average value: 60.1 Grade Count:78
Ball Indentation Hardness 27.0 - 60.0 MPaAverage value: 40.1 MPa Grade Count:13
Tensile Strength, Ultimate 6.89 - 55.2 MPaAverage value: 20.6 MPa Grade Count:106
 18.0 - 34.0 MPa
@Temperature 100 - 100 °C
Average value: 26.5 MPa Grade Count:2
Tensile Strength, Yield 10.0 - 23.5 MPaAverage value: 17.0 MPa Grade Count:9
Elongation at Break 2.00 - 450 %Average value: 221 % Grade Count:111
 5.80 - 8.70 %
@Temperature 100 - 100 °C
Average value: 7.57 % Grade Count:2
Modulus of Elasticity 0.0931 - 4.32 GPaAverage value: 1.36 GPa Grade Count:26
 0.379212 - 0.489528 GPa
@Temperature 100 - 100 °C
Average value: 0.438 GPa Grade Count:2
Flexural Yield Strength 4.12 - 103 MPaAverage value: 28.4 MPa Grade Count:15
Flexural Modulus 0.490 - 4.83 GPaAverage value: 1.64 GPa Grade Count:21
Compressive Yield Strength 0.785 - 54.0 MPaAverage value: 14.9 MPa Grade Count:40
 1.80 - 43.0 MPa
@Temperature 100 - 150 °C
Average value: 21.8 MPa Grade Count:4
 1.80 - 43.0 MPa
@Strain 0.200 - 17.6 %
Average value: 21.8 MPa Grade Count:4
Compressive Modulus 0.430 - 2.14 GPaAverage value: 0.875 GPa Grade Count:11
 0.500 - 0.860 GPa
@Temperature 100 - 100 °C
Average value: 0.622 GPa Grade Count:2
Shear Strength 14.479 - 19.9948 MPa
@Temperature 26.7 - 149 °C
Average value: 17.4 MPa Grade Count:1
Izod Impact, Notched 1.10 - 6.67 J/cmAverage value: 2.59 J/cm Grade Count:8
Izod Impact, Unnotched 1.60 J/cmAverage value: 1.60 J/cm Grade Count:10
Coefficient of Friction 0.0600 - 0.540Average value: 0.178 Grade Count:51
Coefficient of Friction, Static 0.0200 - 0.270Average value: 0.108 Grade Count:36
Tear Strength 12.0 - 71.0 kN/mAverage value: 33.9 kN/m Grade Count:5
Peel Strength 0.701 - 5.47 kN/mAverage value: 2.39 kN/m Grade Count:11
 1.38487 - 1.84065 kN/m
@Temperature 288 - 288 °C
Average value: 1.67 kN/m Grade Count:3
 1.38487 - 1.84065 kN/m
@Time 10.0 - 20.0 sec
Average value: 1.67 kN/m Grade Count:3
K (wear) Factor 10.0 - 142 x 10-8 mm³/N-MAverage value: 30.8 x 10-8 mm³/N-M Grade Count:14
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10000 - 1.00e+18 ohm-cmAverage value: 1.74e+17 ohm-cm Grade Count:53
Surface Resistance 1000 - 1.00e+16 ohmAverage value: 1.46e+15 ohm Grade Count:39
Dielectric Constant 1.92 - 11.2Average value: 3.83 Grade Count:30
Dielectric Strength 3.00 - 37.0 kV/mmAverage value: 17.4 kV/mm Grade Count:29
 11.8504 - 12.5197 kV/mm
@Temperature 121 - 121 °C
Average value: 12.2 kV/mm Grade Count:2
 11.8504 - 12.5197 kV/mm
@Time 10800 - 10800 sec
Average value: 12.2 kV/mm Grade Count:2
Dissipation Factor 0.0000100 - 0.420Average value: 0.0225 Grade Count:26
Dielectric Loss Index 0.000630 - 0.390Average value: 0.142 Grade Count:4
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 237 µm/m-°CAverage value: 79.1 µm/m-°C Grade Count:49
 50.0 - 171 µm/m-°C
@Temperature -60.0 - 300 °C
Average value: 107 µm/m-°C Grade Count:16
CTE, linear, Transverse to Flow 63.9 - 84.0 µm/m-°CAverage value: 74.4 µm/m-°C Grade Count:4
 44.0 - 106 µm/m-°C
@Temperature -60.0 - 250 °C
Average value: 73.1 µm/m-°C Grade Count:6
Specific Heat Capacity 0.790 - 1.00 J/g-°CAverage value: 0.910 J/g-°C Grade Count:12
Thermal Conductivity 0.220 - 0.558 W/m-KAverage value: 0.341 W/m-K Grade Count:33
 0.200 - 1.44 W/m-K
@Temperature 80.0 - 250 °C
Average value: 0.480 W/m-K Grade Count:18
Melting Point 327 °CAverage value: 327 °C Grade Count:27
Maximum Service Temperature, Air 230 - 316 °CAverage value: 262 °C Grade Count:52
Deflection Temperature at 1.8 MPa (264 psi) 198 - 260 °CAverage value: 235 °C Grade Count:4
Minimum Service Temperature, Air -268 - -20.0 °CAverage value: -185 °C Grade Count:41
Decomposition Temperature 500 °CAverage value: 500 °C Grade Count:11
Flammability, UL94 V-0Grade Count:36
Oxygen Index 95.0 - 100 %Average value: 95.7 % Grade Count:12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 °CAverage value: 370 °C Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled

O1903 / 77908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.