MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Pressure Seal 19467 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Compound 19467 is a 40 durometer black colored Silicone elastomer. It exhibits good resistance to heat and compression set. It will remain non brittle at very low temperatures.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 8 GE 409 A19 B37 EA14 EO16 EO36 F19 G11; 2 GE 407 A19 B37 EA14 EO16 EO36 F19 G11
ZZ-R-765 Class 2a & 2b Grade 40
A-A-59588 Class 2a & 2b Grade 40
AMS 3301

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 44
 22
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3
 38
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 39
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 44
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
 44
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
 44
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
Tensile Strength 925 psi
 819.5 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 905.6 psi
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 949.1 psi
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
 1078.6 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 563 %
 563 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 592.3 %
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
 621 %
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 644.1 %
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
100% Modulus 111 psi
Tear Strength 81.0 pliDie B
 87.0 pliDie C
Compression Set 7.4 %
@Treatment Temp. 175 °C,
Time 79200 sec
Plied
 9.4 %
@Treatment Temp. 150 °C,
Time 252000 sec
Solid
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -120 °F
Shrinkage 0.60 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 3.6 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 4.3 %
@Treatment Temp. 175 °C,
Time 252000 sec
Volume, ASTM Oil #1
 47.3 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL161 / 318371

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.