MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® Perfluor GA-105 Perfluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® Perfluor GA-105 is a peroxide curable perfluoroelastomer (FFKM). This grade offers good mechanical properties, excellent chemical and solvent resistance as compared with other fluoroelastomers, and can be used for applications under severe conditions. Perfluor GA-105 is also suitable for semiconductor applications due to its high level of cleanliness.

Typical Applications: Semiconductor manufacture, salt electrolytic processes, chemical engineering, analytical instruments, oil and gas, fuel cells, painting and coating equipment, fuel cells, aerospace applications, other

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
Mooney Viscosity 65
@Temperature 100 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 20.0 MPa
Elongation at Break 130 %
100% Modulus 12.0 MPa
@Strain 100 %
Compression Set 15 %
@Temperature 200 °C,
Time 252000 sec
P-24 O-ring, 25% deformation, 30 min recovery
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °Ccontinuous use
 220 °Cpeak for short time
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 min(JRS Type II: 10 mins @160°C), T90
 4.00 hour
@Temperature 180 °C
Post cure
 10.0 min
@Temperature 160 °C
Press Cure
 
Descriptive Properties
ColorWhite or transparent sheet
Detection limit0.5 ppmFe
 0.5 ppmNa
 0.5 ppmCu
 0.5 ppmMg
 0.5 ppmZn
 1.0 ppmAl
Test Formula1 phr2,5-dimethyl-2,5 di-(t-butylperoxy)hexane (100%)
 100 phrBase Polymer
 15 phrCarbon black MT (N-990)
 3 phrTAIC (100%)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® AeroSeal™ 7797 Fluoroelastomer
Freudenberg Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound
AGC AFLAS® PM-1100 TFE/P Perfluoroelastomer
3M Dyneon™ TFE 90 Peroxide Cure Perfluoroelastomer
3M Dyneon™ PFE 80Z Peroxide Cure Perfluoroelastomer

PDAIJ9870 / 209941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.