MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.

Unibar 700-2 can be hardened by conventional methods, to Rc 50 on the bar surface, responds well to austempering (ADI).

Information provided by United Cast Bar Ltd.

Key Words: EN-1563-GJS-700-2 GGG70; Meehanite SP700.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 230 - 305
@Load 3000 kg
10 mm ball
Tensile Strength 660 MPa
@Diameter 105 - 200 mm
 660 MPa
@Diameter 205 - 600 mm
 700 MPa
@Diameter 25.0 - 50.0 mm
 700 MPa
@Diameter 55.0 - 100 mm
Tensile Strength, Yield 380 MPa
@Diameter 105 - 200 mm,
Strain 0.2 %
 380 MPa
@Diameter 205 - 600 mm,
Strain 0.2 %
 400 MPa
@Diameter 55.0 - 100 mm,
Strain 0.2 %
 420 MPa
@Diameter 25.0 - 50.0 mm,
Strain 0.2 %
Elongation at Break 1.0 %
@Thickness 105 - 200 mm
 1.0 %
@Thickness 205 - 600 mm
 2.0 %
@Thickness 25.0 - 50.0 mm
 2.0 %
@Thickness 55.0 - 100 mm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.25 - 3.7 %
Iron, Fe 92.83 - 94.19 %as balance
Magnesium, Mg 0.040 - 0.070 %
Manganese, Mn 0.10 - 0.30 %
Phosphorus, P 0.015 - 0.080 %
Silicon, Si 2.4 - 3.0 %
Sulfur, S 0.0050 - 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Ductile Iron grade 60-40-18

NUNITED09 / 160456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.