MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics RPC™ 2300-W Wet Felt
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Wet Felt is a high-alumina, ceramic fiber material made by a vacuum forming process that produces a unique insulating process capable of withstanding 2300°F (1260°C). Bonded with our standard bond, it has virtually unlimited uses. It is shipped wet in sheets, rolled or flat, and sealed in protective plastic bags. Standard sizes are 48 x 36 x 1/8 to 1" (1200 x 900 x 3.125 to 25mm) thick.

Features:

  • Non-self sticking and can be joined by air-set mortar
  • Drying time is 24 to 48 hours
  • Maintains wet shape and characteristics of prefired material after drying
  • Random fiber orientation and a tightly knit structure
  • Colloidal silica is disbursed uniformly throughout the entire piece and does not drain out
  • Does not require costly dryers, tooling or machining to conform to size requirements
  • Applications:

  • Wrapping exhaust manifolds in marine engines
  • Wrapping fuel injector nozzles in solid fuel fired kilns
  • Lining combustion duct work in incinerators and boilers
  • Lining hot tuyers in upcomers of blast furnaces
  • Hand packed to protect the anchor of an element hanger module
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 71 - 82ASTM D2240
    Modulus of Rupture 0.0560 ksi
    Compressive Yield Strength 0.0500 MPaat 5% deformation
     0.0600 MPaat 10% deformation
     
    Thermal PropertiesOriginal ValueComments
    Specific Heat Capacity 0.270 BTU/lb-°F
    Thermal Conductivity 0.480 BTU-in/hr-ft²-°F
    @Temperature 260 °C
     0.720 BTU-in/hr-ft²-°F
    @Temperature 538 °C
     1.03 BTU-in/hr-ft²-°F
    @Temperature 816 °C
     1.52 BTU-in/hr-ft²-°F
    @Temperature 1090 °C
    Melting Point 3200 °F
    Maximum Service Temperature, Air 2300 °F
    Shrinkage 0.30 %
    @Temperature 816 °C,
    Time 86400 sec
     1.9 %
    @Temperature 982 °C,
    Time 86400 sec
     2.7 %
    @Temperature 1090 °C,
    Time 86400 sec
     3.4 %
    @Temperature 1200 °C,
    Time 86400 sec
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 32 %
    SiO2 68 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM199 / 2519

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.