MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.

Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addition, it has improved resistance to high temperature, and can be used for components which will withstand long-term temperature stresses.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183/A
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 20 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
 20.5 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
 60 cP
@Shear Rate 100 1/s,
Temperature 300 °C
 70 cP
@Shear Rate 100 1/s,
Temperature 290 °C
 100 cP
@Shear Rate 100 1/s,
Temperature 280 °C
 101 cP
@Shear Rate 10 1/s,
Temperature 300 °C
 105 cP
@Shear Rate 10 1/s,
Temperature 290 °C
 120 cP
@Shear Rate 10 1/s,
Temperature 280 °C
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm
Linear Mold Shrinkage, Transverse 0.019 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPaISO 527 Type 1A
Tensile Strength, Yield 90.0 MPaISO 527 type 1 A
Tensile Stress at Strain 30.0 MPa
@Strain 1 %
 58.0 MPa
@Strain 2 %
 78.0 MPa
@Strain 3 %
 85.0 MPa
@Strain 4 %
Elongation at Break 30 %ASTM D638
 50 %ISO 527 Type 1A
Elongation at Yield 4.0 %ISO 527 type 1 A
Tensile Modulus 3000 MPaISO 527 Type 1A
Flexural Strength 120 MPaISO 178
 125 MPaASTM D790
Flexural Modulus 3000 MPaISO 178
 3300 MPaASTM D790
Izod Impact, Notched 80.0 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²ISO 180/1eA
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 4.50 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 2.9IEC 60250
Dielectric Strength 25.0 kV/mmIEC 60243
Dissipation Factor 0.030IEC 60250
Comparative Tracking Index 350 VSolution B; IEC 60112
 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °CASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
1210
 V-2
@Thickness 3.20 mm
1210
Oxygen Index 26 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY

PRHOD655 / 137886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.