MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Polypropylene PPS 15080 S01 is a high melt flow rate homopolymer with a very narrow molecular weight distribution.

Polypropylene PPS 15080 S01 is intended for the extrusion of fine fibers with the melt blown technology.

It can also be used in compounding extrusion applications.

This material is available in pellet form.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Melt Flow 800 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
NatureWorks® Ingeo™ 5051X Fiber Grade PLA
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications
Braskem CP1200B Homopolymer Polypropylene

PTOTAL879 / 130604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.