MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head laminations and magnetometer bobbin cores.

Information provided by Goodfellow.

Key Words: Permalloy C®, Mumetal, Mu-Metal
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 105 - 290
Tensile Strength at Break 530 - 900 MPa
Tensile Modulus 190 - 221 GPa
Izod Impact, Unnotched 0.420 - 1.00 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000550 - 0.0000620 ohm-cm
Magnetic Permeability 60000Initial
 240000Maximum
Magnetic Coercive Force, Hc 0.0126 Oe
Magnetic Remanence, Br 3700 Gauss
Curie Temperature 380 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 30.0 - 35.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 5.0 %
Iron, Fe 14 %
Molybdenum, Mo 4.0 %
Nickel, Ni 77 %
 
Descriptive Properties
Saturation Induction (T)0.77

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Moly Permalloy Electrical Alloy
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy
Special Metals NILOMAG® Alloy 77
Goodfellow Nickel/Iron/Molybdenum Alloy
Aperam Mumetal-pu Bar-Magnetic Alloys application

NGOODF171 / 16241

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.