MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Tantalum, UNS R05200
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Some information provided by California Fine Wire.

Key Words: ASTM B365
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.600 lb/in³
Vapor Pressure 6.298e-9 bar
@Temperature 2351 °C
 7.488e-9 bar
@Temperature 2365 °C
 4.019e-8 bar
@Temperature 2487 °C
 9.82e-8 bar
@Temperature 2566 °C
 1.72e-7 bar
@Temperature 2615 °C
 2.44e-7 bar
@Temperature 2652 °C
 3.703e-7 bar
@Temperature 2675 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 180.94791995
Atomic Number 73
Thermal Neutron Cross Section 21.3 barns/atom
X-ray Absorption Edge 0.18393 ÅK
 1.06084 ÅLI
 1.11264 ÅLII
 1.25427 ÅLIII
Electrode Potential 4.1 V
Electronegativity 1.5Pauling
Ionic Radius 0.680 ÅCrystal Ionic Radius for Valence +5
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 70 - 80Electron beam melted, cold rolled, then annealed at 1200°C
Tensile Strength at Break 50000 psiAnnealed
 75000 psiStress relieved
 100000 psiHard
Tensile Strength, Ultimate 205 - 276 MPaElectron beam melted, cold rolled, then annealed at 1200°C
Tensile Strength, Yield 165 - 180 MPa
@Strain 0.2 %
Electron beam melted, cold rolled, then annealed at 1200°C
Elongation at Break 35 - 70 %Electron beam melted, cold rolled, then annealed at 1200°C
Modulus of Elasticity 179 - 185 GPaElectron beam melted, cold rolled, then annealed at 1200°C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 74.6 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.50 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.138 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 59.4 W/m-K
Melting Point 5234 °F
Boiling Point 5458 °C
Maximum Service Temperature, Air 500 °COperating Temperature
 
Component Elements PropertiesOriginal ValueComments
Tantalum, Ta 99.96 %alternate source states 99.98%
 
Descriptive Properties
MagneticNone
Temperature Coefficient of Resistance0.0038 ohms/ohm-°C0-100°C
Thermal EMF vs. Copper-0.004

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tantalum, Ta; Annealed
Tantalum, Ta; Cold Worked
Tantalum, UNS R05400
H.C. Starck NRC® Tantalum (UNS R05200)
304 Stainless Steel

AMETa02 / 108

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.