MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Platinum Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Platinum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 15.5 - 21.8 g/ccAverage value: 20.3 g/cc Grade Count:105
 
Chemical PropertiesOriginal ValueComments
Thermal Neutron Cross Section 9.00 barns/atomAverage value: 9.00 barns/atom Grade Count:3
Electrode Potential 1.20 VAverage value: 1.20 V Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60.0 - 360Average value: 180 Grade Count:48
Hardness, Knoop 103 - 431Average value: 222 Grade Count:44
Hardness, Rockwell A 42.0 - 70.0Average value: 55.5 Grade Count:35
Hardness, Rockwell B 45.0 - 100Average value: 77.5 Grade Count:33
Hardness, Rockwell C 20.0 - 40.0Average value: 27.4 Grade Count:15
Hardness, Rockwell 15T 60.0 - 97.0Average value: 87.8 Grade Count:16
Hardness, Vickers 40.0 - 378Average value: 167 Grade Count:69
Tensile Strength, Ultimate 125 - 2070 MPaAverage value: 741 MPa Grade Count:81
Tensile Strength, Yield 190 - 1520 MPaAverage value: 651 MPa Grade Count:8
Elongation at Break 0.500 - 35.0 %Average value: 15.8 % Grade Count:63
Modulus of Elasticity 102 - 205 GPaAverage value: 142 GPa Grade Count:12
Poissons Ratio 0.390Average value: 0.390 Grade Count:3
Shear Modulus 56.0 - 62.0 GPaAverage value: 60.0 GPa Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000106 - 0.0000665 ohm-cmAverage value: 0.0000295 ohm-cm Grade Count:81
Magnetic Susceptibility 0.00000110Average value: 0.00000110 Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.70 - 21.0 µm/m-°CAverage value: 12.6 µm/m-°C Grade Count:13
Specific Heat Capacity 0.134 J/g-°CAverage value: 0.134 J/g-°C Grade Count:3
Thermal Conductivity 18.0 - 69.1 W/m-KAverage value: 40.6 W/m-K Grade Count:12
Melting Point 1040 - 2230 °CAverage value: 1750 °C Grade Count:58
Solidus 1040 - 1920 °CAverage value: 1660 °C Grade Count:29
Liquidus 1110 - 1930 °CAverage value: 1690 °C Grade Count:28
Boiling Point 3830 °CAverage value: 3830 °C Grade Count:3
Maximum Service Temperature, Air 350 - 1770 °CAverage value: 1430 °C Grade Count:6
Minimum Service Temperature, Air 50.0 - 1100 °CAverage value: 750 °C Grade Count:3
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.300Average value: 0.300 Grade Count:3
Reflection Coefficient, Visible (0-1) 0.700Average value: 0.700 Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 799 - 1000 °CAverage value: 863 °C Grade Count:7
Casting Temperature 1260 - 2200 °CAverage value: 1630 °C Grade Count:9
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 5.00 - 23.3 %Average value: 11.1 % Grade Count:3
Copper, Cu 0.400 - 5.00 %Average value: 3.10 % Grade Count:4
Gold, Au 5.00 - 85.5 %Average value: 68.6 % Grade Count:6
Indium, In 0.300 - 4.00 %Average value: 1.77 % Grade Count:3
Iridium, Ir 0.100 - 35.0 %Average value: 16.0 % Grade Count:26
Iron, Fe 0.200 %Average value: 0.200 % Grade Count:3
Nickel, Ni 5.00 - 20.0 %Average value: 10.0 % Grade Count:8
Palladium, Pd 4.50 - 40.0 %Average value: 15.5 % Grade Count:9
Platinum, Pt 8.30 - 100 %Average value: 84.3 % Grade Count:107
Rhodium, Rh 0.500 - 40.0 %Average value: 15.6 % Grade Count:22
Ruthenium, Ru 5.00 - 14.0 %Average value: 7.70 % Grade Count:17
Tungsten, W 0.500 - 8.00 %Average value: 5.13 % Grade Count:12
Zinc, Zn 1.50 - 1.80 %Average value: 1.70 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Platinum, Pt, CP Grade, Annealed
Overview of materials for Copper Alloy
Overview of materials for Stainless Steel
Overview of materials for Cast Iron
Overview of materials for Molybdenum Alloy

M01065 / 81696

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.