MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petromont 4101 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, for sewer pipes and for a wide range of profile extrusion applications. It has been specifically designed for corrugated pipes with the addition of colour concentrates.

Petromont HDPE 4101 complies with the material requirements specified by AASHTO M 294. When mixed with an appropriate carbon black masterbatch, Petromont HDPE 4101 black meets the CSA B182.8 standard for use in profile storm sewer pipe and fabricated fittings.

Key Words: Pipe extrusion, corrugated pipe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
Melt Flow 0.22 g/10 minI2; ASTM D1238
 20 g/10 minI21; ASTM D238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 26.2 MPaASTM D638
Elongation at Break >= 600 %ASTM D638
Flexural Modulus 1.17 GPaASTM D790
Tensile Load, Notched Constant >= 24.0 hourSingle Point; ASTM D5397
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -100 °CASTM D746
 
Descriptive Properties
ProcessPipe Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petromont 4100 High Density Polyethylene Resin
Total Finathene® CD 522 HDPE corrugated pipe resin
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)

PPETROM17 / 56211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.