MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Replaced by Propylux VF .

Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer resin, and exhibits better heat and dimensional stability over Propylux.

Applications Include:

  • Tanks/tank covers
  • Food strainers
  • Hot fillers
  • Welding cabinetry
  • Etching rinse tubs
  • Glove Boxes
  • Cutting board
  • Fan shroud and blades

Advantages of Propylux 290:

  • Excellent chemical resistance
  • Lot controlled and traceable
  • Low moisture absorption
  • FDA resin
  • Superior dimensional stability

Information provided by Westlake Plastics Company.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
Water Absorption 0.010 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength at Break 4230 psiASTM D638
Tensile Strength, Yield 4970 psiASTM D638
Elongation at Break 70 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 319 ksiASTM D638
Flexural Strength 9370 psiASTM D790
Flexural Modulus 329 ksiASTM D790
Compressive Yield Strength 6880 psiASTM D695
Izod Impact, Notched 3.00 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.7 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 309 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 201 °FASTM D648
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BP Amoco ACCPRO® 9119X Extrusion Grade Polypropylene
Mitsubishi Chemical Advanced Materials Proteus™ Copolymer PP Natural Polypropylene
Westlake Plastics Propylux® HS Polypropylene-heat stabilized For Medical Applications
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene

PWEST991 / 131201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.