MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Xytron™ G3080E PPS-I-GF30 Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

Material Notes: Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.

Features: 30% Glass Reinforced. Improved Impact. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 48.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 63.0 MPa
@Temperature 120 °C
ISO 527-1/-2
 140 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Elongation at Break 2.5 %
@Temperature 23.0 °C
ISO 527-1/-2
 6.8 %
@Temperature 120 °C
ISO 527-1/-2
 8.5 %
@Temperature 160 °C
ISO 527-1/-2
 9.0 %
@Temperature 200 °C
ISO 527-1/-2
Tensile Modulus 1900 MPa
@Temperature 200 °C
ISO 527-1/-2
 2500 MPa
@Temperature 160 °C
ISO 527-1/-2
 4500 MPa
@Temperature 120 °C
ISO 527-1/-2
 9300 MPa
@Temperature 23.0 °C
ISO 527-1/-2
Flexural Modulus 2000 MPa
@Temperature 200 °C
ISO 178
 2800 MPa
@Temperature 160 °C
ISO 178
 6800 MPa
@Temperature 120 °C
ISO 178
 7900 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 16.5 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Dielectric Strength 36.0 kV/mmIEC 60243-1
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CISO 11359-1/-2
 110 µm/m-°Cabove Tg; ISO 11359-1/-2
CTE, linear, Parallel to Flow 14.0 µm/m-°Cabove Tg; ISO 11359-1/-2
 18.0 µm/m-°CISO 11359-1/-2
Melting Point 280 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7960 / 291396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.