MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/420 Thermoset Elastomer (TSE)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polidiemme® XLPO -Cross-linkable Polyolefin

Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)

Standard complying

- EN 50363-1 EI7; EN 50363-2 EM6; EN50363-0 G7; Cenelec HD 603 DIH1, DIH2 and DIH3; BS 7655 GP4, GP5. GP6 and GP7; IEC 60092/360 EPR and HEPR; IEC 60502 EPR and HEPR; VDE 0207/20 3GI3

Crosslinkable; Low Toxicity

Uses: Low Voltage Insulation; Power Cable Jacketing; Wire & Cable Applications

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D792
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 32ISO 868
Tensile Strength at Break 20.5 MPaASTM D638
Elongation at Break 470 %ASTM D638
Tensile Modulus 7.00 MPaISO 527-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.30e+15 ohm-cm
@Temperature 90.0 °C
ASTM D257
 4.10e+15 ohm-cm
@Temperature 20.0 °C
ASTM D257
Dielectric Constant 2.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 39.0 kV/mmASTM D149
Dissipation Factor 0.00080
@Frequency 1000 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Zone 1 140 - 160 °C
Zone 2 150 - 170 °C
Zone 3 160 - 180 °C
Zone 4 170 - 190 °C
Die Temperature 180 - 220 °C
 
Descriptive Properties
IRHD Hardness91ASTM D1415
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidiemme® G/450 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/220 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Polidiemme® G/440 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Catalyst Masterbatch CT/2 Polyolefin
Syensqo (Solvay Specialty Polymers) Catalyst Masterbatch CT/2-HP Polyolefin

PSOL8Y6318 / 193239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.