MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Versify™ 2400 Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Versity™ 2400 Elastomer is a resin with a low melt flow rate making it suitable for extrusion and calendaring processes. It has excellent compatibility with PP and is useful agent to bring softness and temperature performance.
Main Characteristics:
  • Pellet
  • Low Melt Flow Rate
  • Free Flowing
  • Compatible with PP
  • Soft polypropylene
  • Low Crystallinity
Applications:
  • Membranes
  • Highly filled compounds
  • Extrusion Applications
Compiles with: US FDA 21 CFR 175.105©(5); EU No 10/2011; US FDA FCN 909

Availability: Asia Pacific; Europe; Latin America; North America

Agency Ratings: FDA 21 CFR 175.105©(5); FDA FCN 909; EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.865 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Crystallinity 12 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
@Time 10.0 sec
Compression Molded; ASTM D2240
Hardness, Shore D 26
@Time 10.0 sec
Compression Molded; ASTM D2240
Tensile Strength at Break 870 psiCompression Molded; ASTM D638
Elongation at Break 11 %Compression Molded; ASTM D638
Flexural Modulus 3700 psi1% Secant, Compression Molded; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 108 °FASTM D1525
Glass Transition Temp, Tg -22.0 °F
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %
@Thickness 2.00 mm
Injection Molded; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF579 / 311272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.