MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® Care ML-GB30 Nylon 12, 30% Glass Bead Filled, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Glass Bead Filled

Material Notes: Microglass bead-filled (30%) PA12 resin for the injection molding of rigid, low-warpage and dimensionally accurate moldings
Industrial Sector: Sustainable, Industry and Engineering, Medical Devices
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Conformity: Biocompatibility, Medical application
Additives: Glass beads / spheres
Applications: Encapsulation
Regulatory: US Pharmacopeia Class VI conformity

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
Water Absorption 0.0110 %Sim to ISO 62
Moisture Absorption 0.00500 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00600 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00700 cm/cmISO 294-4, 2577
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 37.0 MPaISO 527
Tensile Strength 47.0 MPaISO 527
Tensile Strength, Yield 47.0 MPaISO 527
Elongation at Break 20.0 %Nominal; ISO 527
Elongation at Yield 5.00 %ISO 527
Tensile Modulus 2100 MPaISO 527
Charpy Impact Unnotched 160 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
 160 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 4.40 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm?V; IEC 62631-3-1
Dielectric Constant 3.50
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 4.10
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 36.0 kV/mm
@Thickness 1.00 mm
AC, S20/S20, t.; IEC 60243-1
Dissipation Factor 0.0230
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0310
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
 130 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 178 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2
Vicat Softening Point 155 °C
@Load 5.10 kg
50 K/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CInjection Molding; ISO 294
 250 °C
Mold Temperature 80.0 °CInjection Molding; ISO 294
 80.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
Hold Pressure 70.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption23.9 kgISO 14040, 14044
Global Warming Potential2.4 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 4.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 4.9 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7878 / 325010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.