MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: PC+ABS; Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Linear Mold Shrinkage 0.004 - 0.007 cm/cm0.004 - 0.007 in/inASTM D955
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 260 °C
15 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa
@Thickness 3.17 mm
8700 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 50 %
@Thickness 3.17 mm
50 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 89.0 MPa
@Thickness 3.17 mm
12900 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.57 GPa
@Thickness 3.17 mm
373 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL File E155285
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 266 °C450 - 510 °F
Middle Barrel Temperature 246 - 274 °C475 - 525 °F
Front Barrel Temperature 246 - 288 °C475 - 550 °F
Nozzle Temperature 246 - 288 °C475 - 550 °F
Melt Temperature 246 - 288 °C475 - 550 °F
Mold Temperature 57.2 - 85.0 °C135 - 185 °F
Drying Temperature 96.1 °C205 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.9 - 110 MPa10000 - 16000 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Screw Speed 25 - 75 rpm25 - 75 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant
Chi Mei Kibilac® PW-978B ASA, High Heat
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
Covestro Bayblend® FR3010 HF PC/ABS Blend

PZ9PU42qv / 146987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.