MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2800 B-75A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D 792
Linear Mold Shrinkage 0.013 - 0.016 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7510 s delay; ASTM D 2240
Tensile Strength at Break 1000 psi
@Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
Tensile Stress at Strain 430 psi
@Strain 50 %,
Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
 520 psi
@Strain 100 %,
Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
 780 psi
@Strain 100 %,
Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
Elongation at Break 750 %
@Thickness 3.17 mm
Die C; 20 in/min (500 mm/min); ASTM D412
Tear Strength 185 pliDie C; ASTM D 624
Compression Set 30 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 48 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; Type 2; ASTM D 395
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 440 °F
Mold Temperature 50.0 - 175 °F
Drying Temperature 175 °F
Dry Time 2 - 3 hour
Moisture Content <= 0.080 %
Dew Point 0.000 °F
Injection Pressure 10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE))
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
RTP Company RTP 2800 D-75A Thermoplastic Polyolefin Elastomer (TEO)
RTP Company ESD A 2800 B-75A Black Thermoplastic Polyolefin Elastomer (TEO) ESD Protection - Static Dissipative
RTP Company EMI 2863-75A Thermoplastic Polyolefin Elastomer (TEO), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

PQZWA2703 / 91312

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.