CALIBRE™ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical storage discs (CD-R, CD-RW, DVD, MO and PD). Information provided by Dow |