MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ASTM A470-8 1Cr-1Mo-0.25V STEEL FORGINGS FOR TURBINE ROTORS AND SHAFTS (ASTM A470-8)
Categories: Metal; Ferrous Metal; ASTM Steel

Material Notes:

Creep and rupture data provided by NIMS

Key Words: UNS K23010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Rupture Strength 65.0 - 81.0 MPa
@Temperature 575 °C,
Time 3.60e+8 sec
 116 - 146 MPa
@Temperature 550 °C,
Time 3.60e+8 sec
 178 - 205 MPa
@Temperature 525 °C,
Time 3.60e+8 sec
 228 - 255 MPa
@Temperature 500 °C,
Time 3.60e+8 sec
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 - 0.35 %
Chromium, Cr 0.90 - 1.5 %
Iron, Fe 94.217 - 97.5 %
Manganese, Mn <= 1.0 %
Molybdenum, Mo 1.0 - 1.5 %
Nickel, Ni <= 0.75 %
Phosphorus, P <= 0.015 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.018 %
Vanadium, V 0.20 - 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S1 Tool Steel, quenched 955°C (1750°F), tempered 150°C (300°F)
ASTM A543 Steel, Grade C
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.25 in. round High Strength Alloy Steel
Latrobe Lescalloy® UT-18 VAC-ARC ; 6 in. round High Strength Alloy Steel
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate

NIMS009 / 77526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.