MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 701/60 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: ELASTOSIL® R 701/60 is a non postcure HCR grade for extrusion and molding applications.

Special features:

  • heat- and reversion-stabilized
  • Non-post-cure properties: The differences in the mechanical properties of postcured and non-post-cured vulcanizates are only very slight. When Curing Agent E is used, blooming of the decomposition products will not occur.
  • The compounds may be blended to produce any shore hardness value between 40 and 80. Blends with products from other series are also possible.
  • good resistance to mineral oil
  • high elasticity and very low compression set, even when Curing Agent E is used
Application: The compounds are recommended for all kinds of seals that come into contact with mineral oils. ELASTOSIL® R 701/60 is used especially when low compression set is crucial for achieving good seal properties. The compounds may also be used for making high quality silicone-rubber-covered rolls.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38Lubrizol OS 206 304, resistance 540hr/150°C
 44IRM Oil 903, resistance 72hr/150°C
 54IRM Oil 901, resistance 72hr/150°C
 58DIN 53505 A
Tensile Strength at Break 5.80 MPaLubrizol OS 206 304, resistance 540hr/150°C
 6.60 MPaIRM Oil 903, resistance 72hr/150°C
 7.50 MPaDIN 53504 S1
 8.10 MPaIRM Oil 901, resistance 72hr/150°C
Elongation at Break 296 %IRM Oil 903, resistance 72hr/150°C
 353 %DIN 53504 S1
 377 %IRM Oil 901, resistance 72hr/150°C
 407 %Lubrizol OS 206 304, resistance 540hr/150°C
Rebound 59 %DIN 53512
Tear Strength 18.0 kN/mASTM D624 B
Compression Set 8.0 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
post cured 4h/200°C
 
Descriptive Properties
Appearancebeige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF 2-Ethyl Imidazole
Wacker Elastosil® LR 3003/60 A/B Liquid Silicone Rubber
CHT Group QM 261 60 Shore A, Addition Cure Moldmaking Material
Saint-Gobain COHRlastic® 500 General Purpose Silicone Solid Rubber
Saint-Gobain COHRlastic® 600 General Purpose Silicone Solid Rubber

PWACK9227 / 204756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.