MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Rike Chemical HELI™ HPA-600 PVC Foaming Regulator
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: The HL-series PVC foaming regulators acrylic processing aids and have all characteristics of acrylic processing aids. The only difference between them is that the molecular weight of foaming regulators is much more higher than that of processing aids.

Mechanism of Foaming Regulation

There are three purposes for filling the foaming regulators into PVC foaming products. The first one is to promote the fusion of PVC. The second one is to increase the melt strength of PVC so as to prevent from bubble amalgamation for obtaining even foaming products. The third one is to ensure perfect flow of melt for obtaining good appearance of the products. Owing to the difference of products, equipments for processing, raw materials and lubricant system, we developed several types of foaming regulators to satisfy the different requirements.

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.350 - 0.550 g/cc
Volatiles <= 1.3 %
Particle Mesh Size 30 Mesh<2%
Viscosity Measurement 7.1 - 7.5intrinsic
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSHAN057 / 103447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.