MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm Acrylite® 249 Acrylic Sheet, Aerospace Grade
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Data provided by CYRO Industries

Crosslinked acrylic sheet that is certified to meet or exceed Mil Spec MIL-P-8184E, as a type I, Class 2 material. This spec applies to optical quality acrylic sheet that is superior to conventional acrylic sheet in craze resistance, heat resistance, or water absorption.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.13 %24 hrs, 23°C; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 81.0 MPaASTM D638
Elongation at Break 4.5 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 104 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.47 J/g-°Ctypical of Acrylite® sheet
Thermal Conductivity 0.190 W/m-Ktypical of Acrylite® sheet
Deflection Temperature at 1.8 MPa (264 psi) 112 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 0.70 %Before weathering. ASTM D1003
 1.0 %After 10 days accelerated weathering. ASTM D1003
Transmission, Visible 92 %Before and after 10 accelerated weathering; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Röhm Acrylite® GMS Acrylic Sheet, Aerospace Grade
Röhm Acrylite® 8N Acrylic Polymer
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion
Röhm Acrylite® SG Acrylic Sheet, Sign Grade

PCYR33 / 29172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.