MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mo-Sci Corporation GL-0261 Ni Coated Borosilicate Glass Spheres  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Appearance: Solid borosilicate glass microspheres with metallic nickel coating

Typical applications of GL-0261 glass microspheres include: conductive filler for plastic, pigment, and etc.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.20 g/cc0.0434 lb/in³of Dry Beads
Density 2.20 - 2.30 g/cc0.0795 - 0.0831 lb/in³
pH 7.07.0in water
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 0.000600 ohm-cm>= 0.000600 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.20 µm/m-°C
@Temperature 30.0 - 300 °C
1.78 µin/in-°F
@Temperature 86.0 - 572 °F
Softening Point 830 °C1530 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 2.0 - 5.0 %2.0 - 5.0 %Glass
B2O3 10 - 15 %10 - 15 %Glass
Na2O 5.0 - 10 %5.0 - 10 %Glass
Nickel, Ni 90 - 95 %90 - 95 %Coating
Phosphorus, P 2.0 - 10 %2.0 - 10 %Coating
SiO2 70 - 80 %70 - 80 %Glass

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
Mo-Sci Corporation GL 0179 Borosilicate glass frit
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres
BNZ Materials Zelie No. 20 Mortar
Morgan Advanced Ceramics Silicon Carbide Ramming Cement CFR 0130 Thermal Ceramic

CMOSCI022 / 137205

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.