MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 8210 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 8210 adhesive is an aqueous (water-based) covercoat adhesive used to bond a variety of elastomers to primed metal during vulcanization. It is composed of mixture of dispersed fillers, resins and lattices in water-based medium. Chemlok 8210 adhesive is recommended for spray and dip application over Chemlok 8007 and Chemlok 8003 water-based primers. When used over these aqueous primers, this adhesive system will also bond cold rolled steel, phosphatized steel, aluminum and other various substrates.

Features: bonds a variety of natural and synthetic elastomers to primed metal, including NR, SBR and Butyl. works well in injection and transfer molding applications; provides excellent prebake resistance. uses water for cleanup while adhesive is still wet, eliminating the need for significant solvent inventory. provides excellent resistance to hostile environments including salt water and heat. ready to use directly out of the container without dilution; not prone to hard settling; easily redispersed.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 - 9.35 lb/gal
Solids Content 26 - 29 %by weight
Brookfield Viscosity 200 - 500 cP
@Temperature 25.0 °C
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsDeionized water, Propylene Glycol Monomethyl Ether

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9019 / 232408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.