MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Aquathene PM 92949C
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: The Aquathene product line encompasses the Wire & Cable moisture cross-linkable system used in a variety of power cable applications; these include ethylene vinyl silane copolymers along with the complementary catalyst, flame retardant and black master batches, with applications ranging from low voltage insulations to medium voltage jacketing. 

Aquathene PM92949C is a black master batch selected for moisture cure applications. PM92949C contains a 40% loading of a fine particle size carbon black for UV weather resistance, a processing aid and an antioxidant to ensure long-term stability and enhance performance. When PM92949C is melt blended with Aquathene AQ120000 and Aquathene CM04482 or Aquathene CM04483 in the correct ratio this formulation is typically used for USE and USE-2 cable applications. Applications: Wire & Cable.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D1505
Carbon Black Loading 40 %ASTM D1603
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
LyondellBasell Aquathene CM 04483
Syensqo (Solvay Specialty Polymers) Polidan® T/A-MD Polyethylene, Crosslinked (XLPE)

PEQT7072 / 218710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.