MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: 30% glass fiber reinforced, flame retardant

Information provided by Beijing Chemical Industry Research Institute (Group)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccASTM D792
Water Absorption 0.060 %24 hr; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 180 MPaASTM D790
Flexural Modulus 8.00 GPaASTM D790
Izod Impact, Notched 80.0 J/m
@Thickness 3.20 mm
ASTM D256
Charpy Impact Unnotched 4.80 J/cm²ISO179
Charpy Impact, Notched 0.900 J/cm²ISO179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 205 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 225 - 250 °C
Nozzle Temperature 240 °C
Mold Temperature 40.0 - 80.0 °C
Injection Pressure 60.0 - 120 MPa
Back Pressure 6.00 - 18.0 MPa
Screw Speed <= 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Beijing Chemical Industry KAIFA® 201-G30 PBT Resin
Aluminum 1050-O
Envalior Pocan® B 3235 000000 PBT, 30% Glass Fiber

PKAIF06 / 48588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.