MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5852 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 5852 is polyether modified siloxane, used in defoamer and textile formulations.

Application: TEGOPREN® 5852 could be used as additive to defoamer formulations in pulp bleach plants. It can also be used as lubricant in textile auxiliary formulations.

Benefits: TEGOPREN® 5852 is free of silicone oils, that means:

  • as additive in defoamer for the bleaching process of pulp it enhances the dispersability of the defoamer and the rinse of water.
  • In textile application it reduces fiber and fiber metal friction in spin finish application.
  • no adverse effect on the finishing process (painting/electroplating, etc.) of the treated parts.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 - 1.03 g/cc
pH 5.5 - 7.5
Viscosity 220 - 380 cP
 
Descriptive Properties
Appearanceliquid, colorless to pale straw
Content100%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5885 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5851 Defoamer
Evonik TEGOPREN® 5863 Defoamer

PEVONIL597 / 196801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.