MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ohara LICGC™ Lithium-Ion Conducting Glass-Ceramic Formed Plates
Categories: Ceramic; Glass; Optical

Material Notes: LICGC™ is a lithium ion conducting glass ceramic that was developed to serve as a true solid state electrolyte or separator in lithium batteries and other electrochemical devices. It has high lithium ion conductivity of 1 to 4 x 10 -4 S/cm at room temperature. LICGC™ has excellent chemical resistance (water and mild acid have minimal influence on the lithium ion conductivity), excellent physical and mechanical properties, is stable in air & water, non-flammable, prevents dendrite penetration, and is supplied as electrolyte / membrane in various sizes. It consists of Li2O-Al2O3-SiO2-P2O5-TiO2.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.05 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 590
Flexural Strength 140 MPa4-point bending strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.20 µm/m-°C
@Temperature 350 - 600 °C
 >= 9.40 µm/m-°C
@Temperature 30.0 - 350 °C
 
Descriptive Properties
Acid Resistance, Powder Method, RA(P)1
Lithium ion conductivity0.00025 to 0.00040 S/cm25°C
Water Resistance, RW(P)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CZOHARA790 / 281629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.