MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borecene Compact™ RM8346RC Black Linear Polyethylene for Rotational Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: Borecene Compact RM8346RC is a third generation linear medium density black polyethylene for rotational molding. Borecene RM8346RC is a special grade, which has passed rigorous tests and can be considered as a possible replacement for crosslinkable polyethylene in many applications. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM8346RC is a black version of Borecene RM8346RC, suitable for fuel tanks. Borecene Compact RM8346 is delivered as new technology powder.

Borecene Compact RM8346RC contains 1.0% Carbon Black, which is compounded into the polymer. In addition the grade contains an UV stabilizer which gives excellent UV-stability. The polymer contains long-term antioxidant.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccBase Resin; ASTM D1505
ESCR 10% Igepal® >= 200 hourARM Method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2800 psiAt 50 mm/min; ASTM D683 IV
Flexural Modulus 81000 psiAt 2 mm/min; ASTM D790
Dart Drop Total Energy 0.3746 ft-lb/mil(-4oF/-20°C); ASTM D3763
Dart Drop 152 g/micronInstrumented Falling Weight (-4°F/-20°C); ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Brittleness Temperature <= -70.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borecene Compact™ RM8346 Black Linear Polyethylene for Rotational Molding
Borealis Borecene Compact™ RM7406 Black Metallocene Linear Polyethylene for Rotational Molding
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding

PBOREA054 / 27361

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.