MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Engage® 8200 Polyolefin Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer applications. They provide good impact properties in blends with polypropylene (PP) and polyethylene (PE), especially in applications requiring slightly higher melt flow. Engage® 8200 and Engage® 8207 also provide high filler loading capability. They have excellent electrical properties, and when cross-linked give exceptional heat aging, compression set, and weather resistance properties. Engage® 8207 is Engage® 8200 with a nominal loose talc coating. The talc is untreated, with a 1 micron particle size. The product form is free-flowing pellets.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 g/ccASTM D792
Mooney Viscosity 8.0
@Temperature 121 °C
ML 1 + 4; ASTM D1646
Melt Index of Compound 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Hardness, Shore D 21ASTM D2240
Tensile Strength, Ultimate 6.90 MPa508 mm/min; ASTM D638
Tensile Strength, Yield 2.10 MPa508 mm/min; ASTM D638
Elongation at Break 1030 %508 mm/min; ASTM D638
2% Secant Modulus 0.0121 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 60.0 °CDSC, 10°C/min; DuPont Test
Brittleness Temperature <= -76.0 °CASTM D746
 
Descriptive Properties
Comonomer Content38 wt%Dow Method (13C NMR/FTIR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® 8150 Polyolefin Elastomer
Dow Engage® 8100 Polyolefin Elastomer
Dow Engage® 8180 Polyolefin Elastomer
Dow Engage® 8130 Polyolefin Elastomer
Dow Engage® 8842 Polyolefin Elastomer

PDVE33 / 34094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.