MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ SC-305 Thermally Conductive Silicone Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone Elastomer, for Thermal Management

Material Notes:

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccSC-305 Resin
 1.50 g/ccSC-305 Hardener
 1.50 g/ccMixed
Water Absorption <= 0.50 %cured
Viscosity 3500 cP
@Temperature 25.0 °C
SC-305 Resin
 3500 cP
@Temperature 25.0 °C
SC-305 Hardener
 3500 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D 2240
Tensile Strength 215 psicured
Elongation at Break 50 %cured; ASTM D 412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.30e+14 ohm-cm
@Temperature 25.0 °C
cured; ASTM D 257
Dielectric Constant 3.2
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured; ASTM D 150
Dielectric Strength 500 V/milcured
Dissipation Factor 0.0080
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°Ccured; ASTM C 864
Thermal Conductivity 0.700 W/m-KLaser Nano Flash Method, cured
Glass Transition Temp, Tg >= -100 °Ccured
 
Processing PropertiesOriginal ValueComments
Working Life 30.0 min
@Temperature 25.0 °C
Mixed
Gel Time 10.0 min
@Temperature 60.0 °C
mixed, cured
Shelf Life 9.00 Month
@Temperature 25.0 °C
each component from date of manufacture
 
Descriptive Properties
AppearanceDark Grey LiquidSC-305 Hardener
 Grey LiquidMixed
 White LiquidSC-305 Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9289 / 232645

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.