MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Delrin Delrin® 500T NC010 POM-I
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Toughened Medium Viscosity Acetal Homopolymer

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Melt Density 1.18 g/cc
@Temperature 205 °C
Water Absorption 0.30 %
@Time 86400 sec
Immersion; Sim. to ISO 62
 0.82 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.210 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4, 2577
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
cm³/10min Volumetric; ISO 1133
 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 79ISO 2039-2
Hardness, Rockwell R 117ISO 2039-2
Ball Indentation Hardness 155 MPaH 961/30; ISO 2039-1
Tensile Strength, Yield 55.0 MPaISO 527-1/-2
Elongation at Break 35 %Nominal; ISO 527-1/-2
Elongation at Yield 18 %ISO 527-1/-2
Tensile Modulus 2300 MPaISO 527-1/-2
Flexural Strength 60.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2100 MPaISO 178
Poissons Ratio 0.39
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 330 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2300 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1200 MPa1000h; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.6
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-1/-2
Vicat Softening Point 140 °C50°C/h, 50N; ISO 306
 172 °C50°C/h 10N; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
IEC 60695-11-10
 HB
@Thickness 1.50 mm
IEC 60695-11-10
Flame Spread 45.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 °COptimum, Injection
 200 - 210 °CRange, Injection
Mold Temperature 50.0 °COptimum, Injection
 40.0 - 60.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.050 %Injection
Hold Pressure 60.0 - 80.0 MPaInjection
 80.0 MPaInjection
Annealing Temperature 160 °COptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Emissions (mg/kg)<8VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.2G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>POM-I<ISO 11469
PolymerPOM-I
Processing Hold Pressure Time (s/mm)7.5Injection
Resin IdentificationPOM-IISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 500T BK602 POM-I
Delrin Delrin® 100STE NC010 POM-HI
DuPont Mobility and Materials Delrin® 500TE NC010 POM-I
Delrin Delrin® 500P NC010 POM
Delrin Delrin® 500TL NC010 POM-SD

PDSX5124 / 197764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.