MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Description: Cell Cast Acrylic

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.20 %24 hr immersion
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9500 psiASTM D638
Tensile Modulus 400000 psiASTM D638
Compressive Modulus 400000 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 0.350 BTU/lb-°F
@Temperature 25.0 °C
Dupont 900 (Therm. An. Cal.)
Thermal Conductivity 1.30 BTU-in/hr-ft²-°FCento-Fitch
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -26.0 °FLowest Temp Tested for Bullet Resistance
Flame Spread 1.2 in/minBurning Rate UL 94 HB; ASTM D635
Flash Point 870 °FSelf Ignition Temperature; ASTM D1929
Smoke Density 5.0Rating (%); ASTM D2843
 <= 8.0Max (%); ASTM D2843
Shrinkage 2.2 %Residual Shrinkage (Internal Strain) Polycast; ASTM D4802
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %As Cast; ASTM D1003
Yellow Index <= 0.70 %As Cast; ASTM D1925
Transmission, Visible >= 90 %As Cast; ASTM D1003
UV Transmittance 0.00 %
@Wavelength 320 nm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 320 °FHot Forming Temperature
 
Descriptive Properties
Ballistic Protection9 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Spartech Polycast UF3 Cell Cast Acrylic
Spartech Polycast SAR (Super Abrasion Resistant) Cell Cast Acrylic
Spartech Polycast Poly II (Mil-P-5425) Cell Cast Acrylic
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic

PSPAR030 / 68471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.